Wyszukaj na stronie

Sea-Line antifouling

The hull was painted follow recommendations of Sea-Line manufacturer. At first layer epoxy primer and then three layers antyfoulingu Sea-Line.

The unit stayed about three months on the rich in algae Lagoon Zegrzyński. Photos illustrate the hull after the season.

“I would recommend Sea-line antifouling :)”

Sea-Line antifouling

Warning: Undefined variable $gallery_style in /home/klient.dhosting.pl/troton/sea-line.eu/public_html/wp-content/themes/Sea-Line/functions.php on line 172

Warning: Undefined variable $gallery_style in /home/klient.dhosting.pl/troton/sea-line.eu/public_html/wp-content/themes/Sea-Line/functions.php on line 172
  • farba jachtowa antyporostowa
  • farba jachtowa antyporostowa
  • farba jachtowa antyporostowa

Do you have questions about "Sea-Line antifouling"

    Also check

    Our FAQ answers to frequently asked questions

    Why the paint does not have the right flow?

    Possible causes

    • No thinning, wrong thinner or wrong amount of thinner
    • Wrong type of roll or brush (wrong bristle lenght)
    • Applying too much or too Little paint,
    • During painting process temperature was too high or the air was too dry,
    • Incorrect preparation of too porous surface,
    • Incorrect proportion of thinner.

    How to prevent

    • Use a brush/Toller suited to the type of surface or paint,
    • Use thinner which is dedicated to the type of application and paints
    • Use thinning proportions which was indicated by manufacturer,
    • Paint in right atmosphere conditions indicated by manufacturer,

    How to remove

    • Grind, clean and paint again.

    Why does the paint have no adhesion?

    Possible causes

    • Wrong surface preparation,
    • Skipping the primer in the system application process,
    • Use of universal thinners or replacements ,
    • Paint incompatibility.

    How to prevent

    • Correct surface preparation (grinding, clearing, degreasing),
    • Use primers which improve adhesion of paints,
    • Use thinners which are dedicated to each paints,
    • Use of paints which are compatible to each other.

    How to remove

    • Grind, clean and paint again.

    Why are the streaks formed?

    Possible causes

    • Wrong viscosity and spraying technique,
    • Failure to maintain proper evaporation time and thickness of layers,
    • Incorrect spraying pressure,
    • Too low temperature of varnish, surface or space ,
    • Wrong thinner or hardener.

    How to prevent

    • Apply the right type of application method indicated by manufacturer,
    • Use working spray guns,
    • Both the object and material must have room temperature of 20ﹾC,
    • Apply correct proportion of base and hardener.

    How to remove

    • Grinding and polishing,
    • Grinding and painting,