GELCOAT FILLER DRY FAST – NEW 2017

In season 2017 Sea-Line  prepared many new products. On of them is Gelcoat Filler DRY FAST. You ask what is the difference between old gelcoat filler and new one ?

Few advanatges:

  • Easy application: hardener is a paste, in the old product hardener was liquid
  • Fast repairs: hardening time it just 4 hours, in the old minimum was 12 hours
  • Selecting the colour to damage: product is available in two colours RAL 9010 and RAL 9001
  • More for less: New gelcoat filler Dry Fast  is available in volume 250 g, old one was 200 g
GELCOAT FILLER DRY FAST – NEW 2017

Also check

Our FAQ answers to frequently asked questions

Can I add more hardener to speed up the reaction?

Do not add more hardener, because after the base has cured, the remaining hardener will react with subsequent layers, which will be applied to the surface and cause defects. For the product to work properly, please follow the proportions given by the manufacturer.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.

Why despite the use of antifouing paint the bottom of the boat is overgrown?

Possible causes

  • Too thin layer of antifouling paint,
  • Choosing the wrong antifouling to type of a boat or yacht
  • Thinning of antifouling paint,
  • Incorrect surface preparation before antifouling application.

How to prevent

  • Apply the right layer thickness of paint indicated by manufacturer,
  • Choose antifouling dedicated to type of boat or yacht and suitable for the type of water,
  • Do not thin antifouling because of the risk of reducing effectiveness,
  • Careful surface preparations (grinding, clearing, degreasing),

How to remove

  • Wet grinding, apply new layers of antifouling paint.