Wyszukaj na stronie

New shades of gelcoat filler for small repairs

We are happy to introduce in Sea-Line offer five new gelcoat filler shades:

  • Dark blue, item number 13973
  • Light gray 06, article number 13972
  • Ivory 04 article number 13970
  • Warm white 03 article number 13971
  • Cool white 02 article number 13974
  • Our basic colors are still available:
  • Cream 05 RAL 9001 No. article 11296
  • Pure white 01 RAL 9010 no. article 11203

To make the selection of the color easier, we marked fillers with a scale from 01 to 06. Number 01 means the lightest shade of white, and 06 is the darkest. To make shade choice easier we supply nautical stores which offer our products with gelcoat samples board.

New shades of gelcoat filler for small repairs

How does DRY FAST gelcoat filler differ from the competition?

  • Convenient application: the hardener is in the form of a paste that is easier to mix from the application than the liquid hardener.
  • Quick repair: hardening time is only 4 hours, compared to other products minimum 12 hours.
  • Easy application: the self-smoothing surface guarantees an aesthetic effect of repairs even used in amateur use
  • Easy for polishing: the hardened surface is easy to polish

All Sea-Line gelcoat fillers are available in a capacity of 250g

Also check

Our FAQ answers to frequently asked questions

Do you have to paint the scratched side of the boat?

If the scratches are not deep, then we can renew the scratched side by polishing with Sea-Line polishing pastes. Above the waterline, when the scratches are not deep, the surface can be repaired with a DRY FAST gel coat filler. Deep scratches should be filled with epoxy filler (selected depending on the requirements of the scratched surface), painted with a primer and then painted with topcoat.

Can I add more hardener to speed up the reaction?

Do not add more hardener, because after the base has cured, the remaining hardener will react with subsequent layers, which will be applied to the surface and cause defects. For the product to work properly, please follow the proportions given by the manufacturer.

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.
Wyjście