Wyszukaj na stronie

11 months on Mediterranean Sea

“Overall I’m pleased with the antifouling action. It is true that I do not have too much comparison, because this is my first boat and the first paint.

The whole weed descended without major problems Karcher (weak). Most overgrown with water line from the more sunny and rudder blade. On the upper edge of the even appeared crustaceans. It is the only place around the hull where they were. ”

Bartosz Szymanski, Yacht SASHQA

Photos bottom after 11 months in the Mediterranean Sea

11 months on Mediterranean Sea

Antifouling miesiecy na Morzu Srodziemnym

Antifouling miesiecy na Morzu Srodziemnym

Antifouling miesiecy na Morzu Srodziemnym

Do you have questions about "11 months on Mediterranean Sea"

    Also check

    Our FAQ answers to frequently asked questions

    Why did the polyurethane topcoat become dull?

    Possible causes

    • Too short time for evaporation of the thinner,

    How to prevent

    • Maintain the right conditions for complete evaporation of the thinner,

    How to remove

    • Mat the surface, degrease and apply the paint according to the rule (right conditions and thinning proportions)
    • Polish surface if needed.

    Can I paint a boat, previously painted with 1 component paint, with polyurethane?

    It is not recommended to apply 2K paints over 1K paints. 1K and 2K inks differ in their composition and properties, including hardness, chemical resistance and durability. 1K paints are one-component and dry by evaporating the solvent, while 2K paints are two-component and need to be cured by adding a hardener. Applying 2K paint over 1K paint can cause unpredictable chemical reactions and lead to undesirable effects such as dulling, chipping or flaking of the paint. Therefore, always use paints according to the manufacturer’s instructions and do not mix different types of paints. farby zgodnie z instrukcjami producenta i nie mieszać różnych rodzajów farb.

    Do you have to paint the scratched side of the boat?

    If the scratches are not deep, then we can renew the scratched side by polishing with Sea-Line polishing pastes. Above the waterline, when the scratches are not deep, the surface can be repaired with a DRY FAST gel coat filler. Deep scratches should be filled with epoxy filler (selected depending on the requirements of the scratched surface), painted with a primer and then painted with topcoat.