Wyszukaj na stronie

Yacht Enamel 1k

Topcoat marine paint 1K (single-component), recommended for use above the waterline and for interior spaces of yachts.

ColorCapacityCode
white RAL 9010125 ml300008166
white RAL 9010750 ml300008154
crem RAL 9001750 ml300008152
red RAL 3001750 ml 300008158
blue RAL 5011750 ml300008161
black RAL 9005750 ml 300008163
Yacht Enamel 1k

Application method

By hand:

  • brush
  • roller

Spray:

  • pneumatic spray

Product description "Yacht Enamel 1k"

  • 1-componet synthetic color enamel
  • Available 5 colors in high gloss
  • Recommended for exterior above waterline and interior
  • Can be use on GRP, steel and wood
  • UV resistance and weathering
  • Excellent flow, high hiding power and stability of paint
  • Easy and universal in application process
  • Use Sea-Line 1K Thinner, which provide appropriate parameters of paint – flow and  time of drying.
  • The previous layer: Sea-Line Universal Yachtprimer 1 – component or epoxy primers 2K

Basic information

TypeLaminates GRP, wood, steel
PlaceAbove waterline
FunctionHigh gloss
Applicationbrush, roll, spray gun
ThinningThinner for 1 – component primer, varnisch, enamel
Theoretical coverage for 1l15-16 m2 for 60 μm WFT/ 40 μm DFT
Number of coats1 ÷ 2
Dry to the touch 20°C:3 h
Dry to rain 20°C:6 h
Fully woterprof10 h
Elapsed time before applying next coat:min. 16 h

You have questions about the product - Yacht Enamel 1k

    Also check

    Our FAQ answers to frequently asked questions

    Can I use universal thinner?

    We do not recommend using universal thinners. The use of a thinner with an unknown composition may result in loss of adhesion, lack of proper flow of paint and varnish defects.

    Why the paint does not have the right flow?

    Possible causes

    • No thinning, wrong thinner or wrong amount of thinner
    • Wrong type of roll or brush (wrong bristle lenght)
    • Applying too much or too Little paint,
    • During painting process temperature was too high or the air was too dry,
    • Incorrect preparation of too porous surface,
    • Incorrect proportion of thinner.

    How to prevent

    • Use a brush/Toller suited to the type of surface or paint,
    • Use thinner which is dedicated to the type of application and paints
    • Use thinning proportions which was indicated by manufacturer,
    • Paint in right atmosphere conditions indicated by manufacturer,

    How to remove

    • Grind, clean and paint again.

    Why the epoxy filler does not harden?

    Possible causes

    • Incorrect proportion of base and herdener,
    • Too low temperature of ambient and surface (less than 10ﹾC),
    • Mixing two components from two different manufacturers,

    How to prevent

    • Apply the correct proportions of components
    • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
    • Use base and hardener from the same manufacturer

    How to remove

    • The uncured mass requires complete removal from the surface.
    Wyjście