    Contamination in topcoat paint?

    Possible causes

    • Inaccurate surface cleaning before paint application,
    • Incorrect painting tools preparation (brush and roll),
    • Performing work in a place exposed to constant contact with dust.

    How to prevent

    • Careful surface preparation (grinding, clearing, degreasing),
    • Careful painting tools preparation before use,
    • Maintain clean work environment

    How to remove

    • Grind, clean and paint again.

    Why the epoxy filler does not harden?

    Possible causes

    • Incorrect proportion of base and herdener,
    • Too low temperature of ambient and surface (less than 10ﹾC),
    • Mixing two components from two different manufacturers,

    How to prevent

    • Apply the correct proportions of components
    • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
    • Use base and hardener from the same manufacturer

    How to remove

    • The uncured mass requires complete removal from the surface.

    Do you have to paint the scratched side of the boat?

    If the scratches are not deep, then we can renew the scratched side by polishing with Sea-Line polishing pastes. Above the waterline, when the scratches are not deep, the surface can be repaired with a DRY FAST gel coat filler. Deep scratches should be filled with epoxy filler (selected depending on the requirements of the scratched surface), painted with a primer and then painted with topcoat.