Zabezpieczenie łodzi
11 months on Mediterranean Sea

“Overall I’m pleased with the antifouling action. It is true that I do not have too much comparison, because this is my first boat and the first paint.

The whole weed descended without major problems Karcher (weak). Most overgrown with water line from the more sunny and rudder blade. On the upper edge of the even appeared crustaceans. It is the only place around the hull where they were. ”

Bartosz Szymanski, Yacht SASHQA

Photos bottom after 11 months in the Mediterranean Sea


Μετοχή:

Δείτε επίσης
Άλλα νήματα σε αυτήν την κατηγορία

Οι συχνές ερωτήσεις μας
Απαντήσεις σε συνήθεις ερωτήσεις

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.

Can I degrease surfaces with acetone?

We do not recommend degreasing the surface with acetone, because acetone evaporates very quickly, which affects the quality of cleaning the painted surface.

Can I add more hardener to speed up the reaction?

Do not add more hardener, because after the base has cured, the remaining hardener will react with subsequent layers, which will be applied to the surface and cause defects. For the product to work properly, please follow the proportions given by the manufacturer.