Linguaggio:

New antifouling

Home » Notizie » New antifouling
Zabezpieczenie łodzi
New antifouling

New antifouling and completing the offer

HARD ANTIFOULING  is recommended to protect areas below the water line. Suitable for all kind of motorboats up to 70 knots speed. It can be also used on sailboats.
Recommended for salt, fresh and mixed water. Due to increased hardness is resistance to damage.
HARD ANTIFOULING Sea-Line can be applied on hulls made of laminate, steel, wooden. Don’t use on aluminium.
Paint in colour : red, blue and black in 0,75 l or 2,5 l can.

NEW COLOUR ALUPLUS SELF-POLISHING. For people, who search paint with high  efficiency and for area on big fouling, we recommended self polishing antifouling ALUPLUS. In season 2018 we add to offer colors blue and black. Available packing in can 0,75l and 2,5 l. The output and efficiency of the paint is 30% higher than with traditional products. It can be applied on hulls made of aluminium.

THINNER FOR ANTIFOULING Thinner for antifouling it’s last product in completing the offer antifouling paint. Thinner it’s product for all antifouling paint Sea-Line. We don’t recommended thinning paint more 5%.

nowe kolory antofouling


Condividi:

Vedi anche
Altre discussioni in questa categoria

Le nostre FAQ
Risposte alle domande più frequenti

Why despite the use of antifouing paint the bottom of the boat is overgrown?

Possible causes

  • Too thin layer of antifouling paint,
  • Choosing the wrong antifouling to type of a boat or yacht
  • Thinning of antifouling paint,
  • Incorrect surface preparation before antifouling application.

How to prevent

  • Apply the right layer thickness of paint indicated by manufacturer,
  • Choose antifouling dedicated to type of boat or yacht and suitable for the type of water,
  • Do not thin antifouling because of the risk of reducing effectiveness,
  • Careful surface preparations (grinding, clearing, degreasing),

How to remove

  • Wet grinding, apply new layers of antifouling paint.
  • Use C1 shell and fouling remover.

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.
La nostra offerta
Familiarizzate con la nostra offerta di materiali e vernici per la costruzione di barche
Exit
Przewiń na górę