Wyszukaj na stronie

Epoxy primer in the “Żagle” water sports magazine

Our new epoxy primer in the “Żagle” water sports magazine.

The multifunctional epoxy spray primer was mentioned in the latest issue of the water sports magazine “Żagle + Jachty Motorowe”.

“Excellent marks in the competition “Gwóźdź Targów Wiatr i Woda 2019″ has obtained a new two-component epoxy primer with a multifunctional application offered in a spray (…) The container has a built-in activation system for mixing two components that extends the pot life of up to 48 hours after activation (… ) ”

“Żagle” No. 5 May 2019

Epoxy primer in the “Żagle” water sports magazine

Also check

Our FAQ answers to frequently asked questions

Can I use selfpolishing Sea-Line and HARD Sea-Line antifoulings on aluminium boat?

Sea-Line HARD and Sea-Line self-polishing antifouling are not intended for aluminum surfaces. They include copper oxide, which in contact with aluminum causes galvanic corrosion. Especially on aluminum, we offer ALU-PLUS self-polishing anti-fouling paint, which, in addition to excellent adhesion to aluminum, is also 30% more effective than traditional anti-fouling paints.

Can I add some thinner to antifouling paint?

There is a possibility of thinning antifouling, but we do not recommend this procedure due to the risk of reducing the effectiveness of the paint. If it is necessary to thin the antifouling paint, it is recommended to dilute it to a maximum of 0-5% (by volume).

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.