Traditionally, along with the approaching spring and the upcoming season, we are happy to invite you to visit the Wind and Water Fair.

This year’s edition will take place on March 12-15 at the new location, i.e. at the Global EXPO Trade Fair and Congress Center at ul. Modlińska 6D in Warsaw.

The meeting will be an opportunity to:

  • show how our products work
  • answer your questions about yachting paints and polishing compounds
  • help in the best solutions selection during boat renovations

Gifts are waiting for the users of our products!

See You in Warsaw!

More about event “Wiatr i Woda 2020”

WIND & WATER March 2020

Also check

Our FAQ answers to frequently asked questions

Why despite the use of antifouing paint the bottom of the boat is overgrown?

Possible causes

  • Too thin layer of antifouling paint,
  • Choosing the wrong antifouling to type of a boat or yacht
  • Thinning of antifouling paint,
  • Incorrect surface preparation before antifouling application.

How to prevent

  • Apply the right layer thickness of paint indicated by manufacturer,
  • Choose antifouling dedicated to type of boat or yacht and suitable for the type of water,
  • Do not thin antifouling because of the risk of reducing effectiveness,
  • Careful surface preparations (grinding, clearing, degreasing),

How to remove

  • Wet grinding, apply new layers of antifouling paint.
  • Use C1 shell and fouling remover.

Can I purchase products directly from you?

We do not sell retail. Our products can be found in many stores in Poland and abroad. Our distributors run stationary and online stores. The full list of distributors and contacts can be found on our website at the following link click here.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.