    Why despite the use of antifouing paint the bottom of the boat is overgrown?

    Possible causes

    • Too thin layer of antifouling paint,
    • Choosing the wrong antifouling to type of a boat or yacht
    • Thinning of antifouling paint,
    • Incorrect surface preparation before antifouling application.

    How to prevent

    • Apply the right layer thickness of paint indicated by manufacturer,
    • Choose antifouling dedicated to type of boat or yacht and suitable for the type of water,
    • Do not thin antifouling because of the risk of reducing effectiveness,
    • Careful surface preparations (grinding, clearing, degreasing),

    How to remove

    • Wet grinding, apply new layers of antifouling paint.
    • Use C1 shell and fouling remover.

    Why the paint does not have the right flow?

    Possible causes

    • No thinning, wrong thinner or wrong amount of thinner
    • Wrong type of roll or brush (wrong bristle lenght)
    • Applying too much or too Little paint,
    • During painting process temperature was too high or the air was too dry,
    • Incorrect preparation of too porous surface,
    • Incorrect proportion of thinner.

    How to prevent

    • Use a brush/Toller suited to the type of surface or paint,
    • Use thinner which is dedicated to the type of application and paints
    • Use thinning proportions which was indicated by manufacturer,
    • Paint in right atmosphere conditions indicated by manufacturer,

    How to remove

    • Grind, clean and paint again.

    Why the epoxy filler does not harden?

    Possible causes

    • Incorrect proportion of base and herdener,
    • Too low temperature of ambient and surface (less than 10ﹾC),
    • Mixing two components from two different manufacturers,

    How to prevent

    • Apply the correct proportions of components
    • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
    • Use base and hardener from the same manufacturer

    How to remove

    • The uncured mass requires complete removal from the surface.