Wyszukaj na stronie

Gelcoat White

Gelcoat based on IZO/NPG resin, thanks to which it achieves good resistance to weather conditions and high mechanical properties. Primarily recommended for repairing minor scratches and for the production of laminate products.

The product is delivered without hardener, you need Metox 30. The gelcoat and the catalyst should be mixed gently.

ColorWeightCode
RAL 9010 white1kg300010262
RAL 9010 white250g300010263
METOX 3020 ml300010282
Paraffin corrector60 ml300010264
Gelcoat White

Color

  • white

Application method

Manually:

  • brush

Product description "Gelcoat White"

It is a gelcoat in RAL 9010 color for versatile use:

  • It is useful both in construction and during repairs of damaged boat elements.
  • It is recommended primarily for lamination.
  • In combination with paraffin corrector, it is used to repair minor scratches.
  • Component A is white, and the hardener is Metox 30 liquid.
  • Mixing proportions of the ingredients “gelcoat”: hardener 100:3.

Important

The package contains only gelcoat.
The hardener and paraffin corrector must be purchased separately.

Basic information

Surface laminat,
Place above and below water line
Function laminating, small repairs
Number of Coats according need
Pot Life 15-25 min in temperature 20°C
Hardening time 24 h in temperature  around 20°C
Color white RAL 9010

Surface preparation

How to use:

First of all, the surface should be degreased and sanded with sandpaper. Remove dust and degrease again.

Mix the base with the hardener in a ratio of 100:3. The gelling time, the so-called potlife, i.e. the possibility of use after mixing the components, is approximately 15-25 minutes at a temperature of approximately 20°C.

Further work:

As already mentioned, the gelcoat undergoes oxygen inhibition under the influence of oxygen (it does not dry out, the surface is always sticky). Assuming that in the case of repairs we use the so-called Topcoat can be achieved by adding paraffin concealer. Recommended amount of paraffin corrector 2%-5%.

You have questions about the product - Gelcoat White

    Gelcoat do laminowania i napraw

    Gelcoat do laminowania i napraw

    Gelcoat do laminowania i napraw

    Also check

    Our FAQ answers to frequently asked questions

    Why the epoxy filler does not harden?

    Possible causes

    • Incorrect proportion of base and herdener,
    • Too low temperature of ambient and surface (less than 10ﹾC),
    • Mixing two components from two different manufacturers,

    How to prevent

    • Apply the correct proportions of components
    • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
    • Use base and hardener from the same manufacturer

    How to remove

    • The uncured mass requires complete removal from the surface.

    Contamination in topcoat paint?

    Possible causes

    • Inaccurate surface cleaning before paint application,
    • Incorrect painting tools preparation (brush and roll),
    • Performing work in a place exposed to constant contact with dust.

    How to prevent

    • Careful surface preparation (grinding, clearing, degreasing),
    • Careful painting tools preparation before use,
    • Maintain clean work environment

    How to remove

    • Grind, clean and paint again.

    Can I paint a boat, previously painted with 1 component paint, with polyurethane?

    It is not recommended to apply 2K paints over 1K paints. 1K and 2K inks differ in their composition and properties, including hardness, chemical resistance and durability. 1K paints are one-component and dry by evaporating the solvent, while 2K paints are two-component and need to be cured by adding a hardener. Applying 2K paint over 1K paint can cause unpredictable chemical reactions and lead to undesirable effects such as dulling, chipping or flaking of the paint. Therefore, always use paints according to the manufacturer’s instructions and do not mix different types of paints. farby zgodnie z instrukcjami producenta i nie mieszać różnych rodzajów farb.