Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.

Is it necessary to always sand the surface between application of two different products?

We recommend to always sand the surface between applying two different products to ensure uniform surface roughness and adhesion of subsequent layers. The sanded surface should also be cleaned and degreased.

Can I purchase products directly from you?

We do not sell retail. Our products can be found in many stores in Poland and abroad. Our distributors run stationary and online stores. The full list of distributors and contacts can be found on our website at the following link click here.