Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,

Is it necessary to always sand the surface between application of two different products?

We recommend to always sand the surface between applying two different products to ensure uniform surface roughness and adhesion of subsequent layers. The sanded surface should also be cleaned and degreased.