We starting new year with new product – polishing compound S08 INDUSTRIAL FORCE CUT.

Why S08 INDUSTRIAL FORCE CUT ?
This polishing compound have one the highest cut level, it allows to remove defects after using sand paper P600. It can be used on hardest surfaces, finished products made of laminate and for molds. Polishing compound will be especially used for light-colored surface.

For whom S08 INDUSTRIAL FORCE CUT ?
S08 INDUSTRIAL FORCE CUT was designed for manufacture which want to in fast way prepare products for next stage of productions.

Advantages S08 INDUTRIAL FORCE CUT :

All details about product are HERE (click)


Μετοχή:

Δείτε επίσης
Άλλα νήματα σε αυτήν την κατηγορία

Οι συχνές ερωτήσεις μας
Απαντήσεις σε συνήθεις ερωτήσεις

Can I use selfpolishing Sea-Line and HARD Sea-Line antifoulings on aluminium boat?

Sea-Line HARD and Sea-Line self-polishing antifouling are not intended for aluminum surfaces. They include copper oxide, which in contact with aluminum causes galvanic corrosion. Especially on aluminum, we offer ALU-PLUS self-polishing anti-fouling paint, which, in addition to excellent adhesion to aluminum, is also 30% more effective than traditional anti-fouling paints.

Why the paint does not have the right flow?

Possible causes

  • No thinning, wrong thinner or wrong amount of thinner
  • Wrong type of roll or brush (wrong bristle lenght)
  • Applying too much or too Little paint,
  • During painting process temperature was too high or the air was too dry,
  • Incorrect preparation of too porous surface,
  • Incorrect proportion of thinner.

How to prevent

  • Use a brush/Toller suited to the type of surface or paint,
  • Use thinner which is dedicated to the type of application and paints
  • Use thinning proportions which was indicated by manufacturer,
  • Paint in right atmosphere conditions indicated by manufacturer,

How to remove

  • Grind, clean and paint again.

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.