Language:

Polyester resin

Home » Products » Resins and repair kit » Polyester resin
Farby antyporostowe
Polyester resin

To obtain a fully-fledged and adequately strong laminate, use a 2:1 weight ratio of resin to glass mat for polyester or a 1:1 weight ratio of resin to glass fabric.To finish laminated surfaces we recommend using Sea-Line® fillers, Sea-Line® epoxy primers, Sea-Line® topcoats or a Sea-Line® gelcoat repair kit.


TypeLaminates, steel
PlaceAbove and below waterline
FunctionLaminating, repairs, reinforcement, gluing
ApplicationBrush, roll
ThinningNot recommended
 Theoretical coverage for 1kg

(for 1 layer laminate)

performance for layer of laminate based on glass fibre mats
150 g/m²

300 g/m²

450 g/m²

~3,5 m²

~1,7 m²

~1,1 m²

performance for layer of laminate based on glass fibre
200 g/m²

400 g/m²

~5 m²

~2,5 m²

Coats numberAccording to your needs
Pot life 20°C10~15 min
Hardening time45 min
Colortransparent
Packcode
250 g

500 g

1 kg

2392

6080

2480

The resin is available in 2 sets:

Set of 250 g
contains a polyester structural resin with hardener, fibre glass mat (0,25m2), disposable gloves, a brush and a cup with a scale for easy dosing of ingredients and instructions for repair.
Set of 500 g
contains a polyester structural resin with hardener and a cup with a scale for easy dosing of ingredients and instructions for repair.

Set of 1 kg
contains a polyester structural resin with hardener and a cup with a scale for easy dosing of ingredients and instructions for repair.


Share:

Do you have any questions?
We will respond as soon as possible
 
See also
Other products in this category

Our FAQ
Answers to frequently asked questions

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,
  • Grinding and painting,

Can I use universal thinner?

We do not recommend using universal thinners. The use of a thinner with an unknown composition may result in loss of adhesion, lack of proper flow of paint and varnish defects.

Contamination in topcoat paint?

Possible causes

  • Inaccurate surface cleaning before paint application,
  • Incorrect painting tools preparation (brush and roll),
  • Performing work in a place exposed to constant contact with dust.

How to prevent

  • Careful surface preparation (grinding, clearing, degreasing),
  • Careful painting tools preparation before use,
  • Maintain clean work environment

How to remove

  • Grind, clean and paint again.
Our offer
Familiarize yourself with our offer of boatbuilding materials and paints
Exit
Przewiń na górę