MS POLYMER on the WiW

Naprawa łodzi

MS POLYMER on the “Wind and Water”

XXX Wind and Water behind us. Among all premiers 2018 we presented MS POLYMER sealing and bonding smart solution. The innovative dispensing solution, combined with the adhesive and sealing parameters of MS POLYMER, was awarded in the category: accessories and equipment.

Wyroznienie WiW 2018 dla MS POLYMER


Μετοχή:

Δείτε επίσης
Άλλα νήματα σε αυτήν την κατηγορία

Οι συχνές ερωτήσεις μας
Απαντήσεις σε συνήθεις ερωτήσεις

Can I purchase products directly from you?

We do not sell retail. Our products can be found in many stores in Poland and abroad. Our distributors run stationary and online stores. The full list of distributors and contacts can be found on our website at the following link click here.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.

Why are the streaks formed?

Possible causes

  • Wrong viscosity and spraying technique,
  • Failure to maintain proper evaporation time and thickness of layers,
  • Incorrect spraying pressure,
  • Too low temperature of varnish, surface or space ,
  • Wrong thinner or hardener.

How to prevent

  • Apply the right type of application method indicated by manufacturer,
  • Use working spray guns,
  • Both the object and material must have room temperature of 20ﹾC,
  • Apply correct proportion of base and hardener.

How to remove

  • Grinding and polishing,