In the April-May issue of magazin Wind, you will find a guide text on the prevention and treatment of osmosis using Sea-Line products.An old proverb says that prevention is better than cure, so we highly recommend reading not only to those who already struggle with osmosis on the hull.In the printed version, you can find Wiatr in most nautical shops and marinas, and always online http://magazynwiatr.pl/archiwum/

 


Μετοχή:

Δείτε επίσης
Άλλα νήματα σε αυτήν την κατηγορία

Οι συχνές ερωτήσεις μας
Απαντήσεις σε συνήθεις ερωτήσεις

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.

Can I purchase products directly from you?

We do not sell retail. Our products can be found in many stores in Poland and abroad. Our distributors run stationary and online stores. The full list of distributors and contacts can be found on our website at the following link click here.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.