Lengua:

MASILLAS DE POLIÉSTER: UNIVERSAL, LIGERA, CON FIBRA DE VIDRIO

Página web » Productos » Masillas » MASILLAS DE POLIÉSTER: UNIVERSAL, LIGERA, CON FIBRA DE VIDRIO
Naprawa łodzi
MASILLAS DE POLIÉSTER: UNIVERSAL, LIGERA, CON FIBRA DE VIDRIO


Tipo de embarcaciónlaminado, madera, acero, aluminio
LugarPor encima por debajo de la linea de flotación
FunciónReparaciones por encima de la linea de flotación y en exterior
AplicaciónA mano/ éspatula
Tiempo de trabajo 20°C3-5 min
Tiempo de secado 20°C20 ± 30 min
Color :
UNIVERSAL

LIGERA

CON FIBRA DE VIDRIO

Blanco

Crema

Marrón

EMBALAJE :

MASILLAS DE POLIÉSTER

UNIVERSAL :

MASILLAS DE POLIÉSTER

LIGERA :

MASILLAS DE POLIÉSTER

FIBREGLASS :

Información técnica:

MASILLAS DE POLIÉSTER

MASILLAS DE POLIÉSTER (low styrene)

Polyester filler universal

Polyester filler lightweight

Polyester filler with fiberglass

Polyester filler universal

Polyester filler with fiberglass


Compartir:

¿Tienes alguna pregunta?
Le responderemos lo antes posible

Productos relacionados

de MASILLAS DE POLIÉSTER: UNIVERSAL, LIGERA, CON FIBRA DE VIDRIO


Ver también
Otros productos de esta categoría

Nuestras FAQ
Respuestas a las preguntas más frecuentes

Why does the paint have no adhesion?

Possible causes

  • Wrong surface preparation,
  • Skipping the primer in the system application process,
  • Use of universal thinners or replacements ,
  • Paint incompatibility.

How to prevent

  • Correct surface preparation (grinding, clearing, degreasing),
  • Use primers which improve adhesion of paints,
  • Use thinners which are dedicated to each paints,
  • Use of paints which are compatible to each other.

How to remove

  • Grind, clean and paint again.

Can I paint the bottom of the boat with polyurethane paint?

Yes, you can paint the bottom of the boat with polyurethane paint due to its high mechanical strength. We recommend this solution when the boat is not launched for a long time and is not exposed to fouling.

Why the resin does not harden?

Possible causes

  • Too low temperature of ambitne,
  • Incorrect proportion of base and herdener,
  • Mixing two components from two different manufacturers

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during whole hardening process,
  • Mix the products thoroughly and bleed the mixture.

How to remove

  • The uncured mass requires complete removal from the surface.
Nuestra oferta
Consulte nuestra oferta de materiales y pinturas para la construcción de embarcaciones
Exit
Przewiń na górę