Linguaggio:

Osmosis repair – EPOXY PRIMER HS 3:2

Home » Recensioni » Osmosis repair – EPOXY PRIMER HS 3:2
Szpachlówki i podkłady szkutnicze
Osmosis repair – EPOXY PRIMER HS 3:2

The next layer isantiosmoticHSEpoxy Primer Sea-Line. It is verydense, you have to get used toher characterand learnto imposeequallayerswith a roller.Withthree layersshouldgo.Certainlymoreamazedpeoplewould achievebetter effect,butfor a firstcontactwith this type ofworkthe end resultwas verysatisfactory. Thanks largely tothe paint, which does not dripso easyandgoodspillsto forma uniform layer.

Full reportofrenovationJakubaMitki

Description ofrepaircan be found at: http://kluczka.pl/blog/
andin the journalYacht-Market,March 2015


Condividi:

Vedi anche
Altre discussioni in questa categoria

Le nostre FAQ
Risposte alle domande più frequenti

Can I use universal thinner?

We do not recommend using universal thinners. The use of a thinner with an unknown composition may result in loss of adhesion, lack of proper flow of paint and varnish defects.

Can I degrease surfaces with acetone?

We do not recommend degreasing the surface with acetone, because acetone evaporates very quickly, which affects the quality of cleaning the painted surface.

Why the epoxy filler does not harden?

Possible causes

  • Incorrect proportion of base and herdener,
  • Too low temperature of ambient and surface (less than 10ﹾC),
  • Mixing two components from two different manufacturers,

How to prevent

  • Apply the correct proportions of components
  • Maintain steady temperature (around 20ﹾC) during the whole hardening process,
  • Use base and hardener from the same manufacturer

How to remove

  • The uncured mass requires complete removal from the surface.