DESCRIZIONE DEL PRODOTTO :

Per ottenere una laminazione di massima qualità e adeguata durezza usare una miscelazione 2:1 in peso per la fibra di vetro mate, se si utilizza il tessuto di vetro miscelare in rapporto 1:1 in peso.


INFORMACIONI DI BASE:

Tipolaminazione, legno, alluminio, acciaio
Postosotto e sopra la linea di gallegg
Utilizzolaminatura

sigillatura

uniformare la superfice

incollare e collegare vari elementi alla struttura

Resa teorica 1 KGTESSUTO MATE
150 g/m²

300 g/m²

450 g/m²

~3,3 m²

~1,7 m²

~1,1 m²

FIBRA DI VETRO
200 g/m²

400 g/m²

~5 m²

~2,5 m²

Miscelazione a volume100 : 50
Miscelazione a peso100 : 44
Durata della miscela a 23°C45 minutti
Tempo di indurimento a 23°C7 ore

CONFEZIONE :

250 g /  CODICE : 3636 (set)

0,9 kg /  CODICE : 8508 (set)

0,5 kg /CODICE: 8483 (set)

5,0 kg /CODICE: 8506 (comp. A)

             /CODICE: 8507 (comp. B)

IN CONFEZIONI DA :

APPLICAZIONE:

Manualmente:

INFORMAZIONI TECNICHE :


Condividi:

Avete domande?
Ti risponderemo il prima possibile
 
Vedi anche
Altri prodotti in questa categoria

Le nostre FAQ
Risposte alle domande più frequenti

Can I add some thinner to antifouling paint?

There is a possibility of thinning antifouling, but we do not recommend this procedure due to the risk of reducing the effectiveness of the paint. If it is necessary to thin the antifouling paint, it is recommended to dilute it to a maximum of 0-5% (by volume).

Contamination in topcoat paint?

Possible causes

  • Inaccurate surface cleaning before paint application,
  • Incorrect painting tools preparation (brush and roll),
  • Performing work in a place exposed to constant contact with dust.

How to prevent

  • Careful surface preparation (grinding, clearing, degreasing),
  • Careful painting tools preparation before use,
  • Maintain clean work environment

How to remove

  • Grind, clean and paint again.

Can I add more hardener to speed up the reaction?

Do not add more hardener, because after the base has cured, the remaining hardener will react with subsequent layers, which will be applied to the surface and cause defects. For the product to work properly, please follow the proportions given by the manufacturer.

La nostra offerta
Familiarizzate con la nostra offerta di materiali e vernici per la costruzione di barche
Exit
Przewiń na górę